Description
This process significantly reduces the time required for polishing, grinding and shaping, allowing parts to be manufactured to precise dimensions prior to heat treatment without concerns of dimensional changes due to scaling, pitting or decarburization. The method is exceptionally straightforward, applicable for both hardening and annealing. Begin by heating the workpiece to approximately 500 deg F, apply the dry compound powder, continue heating to the desired temperature and then quench or cool as necessary. The parts can be cleaned effectively in boiling water.